Attenuation Mechanism and Improvement Strategy of Heterojunction Module (2): Enhancement of Light Injection Annealing, Light Attenuation and Dark Attenuation

2026-11-27 15:54:44

The output power of HJT module is not a fixed value, but will fluctuate dynamically within a certain range with the illumination state and storage conditions.

The characteristic

of HJT

01 Introduction

Heterojunction (HJT) solar cells, which achieve excellent open-circuit voltage and conversion efficiency by virtue of crystalline silicon/amorphous silicon passivation contact structure, are currently the most concerned high-efficiency This dynamic characteristic is due to the large number of mobile hydrogen atoms in the thin film structure of HJT cells. Illumination, heating and standing without light will change the combination state of active atoms, and then affect the conductivity and efficiency output of the battery.

The previous article has specifically analyzed the damage mechanism of ultraviolet light to the amorphous silicon/crystalline silicon interface. This paper focuses on three other phenomena closely related to the behavior of hydrogen atoms: light injection annealing enhancement, white light illumination attenuation (LID) and dark attenuation, and clarifies the unified physical logic behind the three phenomena and their impact on practical use.

02 Unified mechanism

of HJT metastable state To understand the above three phenomena, we need to grasp a core concept: HJT battery is in a "metastable state".

The so-called metastable state means that the performance state of the battery is not unchanged, but will switch between several relatively stable equilibrium points with the external conditions (light intensity, temperature, time). It is the combination and separation of hydrogen atoms and dopant atoms in the film that drives these switches.

(1) The "breaking" and "closing" of hydrogen bonds: the common root

of all phenomena. The film structure of HJT cells contains a large number of doping atoms, phosphorus (P) and boron (B). These doping atoms are supposed to provide free carriers and enhance the conductivity of the film, but after the preparation is completed, a considerable number of doping atoms are in the state of combining with hydrogen atoms (P-H bond, B-H bond), in a "dormant" state, temporarily losing doping activity.

[Technical details] The combination of P-H and B-H bonds makes the outer electrons of doped atoms occupied by hydrogen atoms, which can not contribute free electrons or holes to the lattice, which is equivalent to the temporary "failure" of doped atoms. This is the same type of hydrogen bond dynamics as the mechanism of Si-H bond cleavage in the UV decay in the previous paper, but the level of influence is different: the UV decay acts on the passivation layer at the crystalline silicon/amorphous silicon interface, while the phenomenon discussed in this paper occurs inside the doped amorphous silicon (microcrystalline silicon) film.

When enough energy is provided by light or high temperature, the P-H and B-H bonds are broken, the doped atoms are reactivated, the conductivity of the film is improved, and the efficiency of the cell is increased, which is the fundamental reason for the enhancement of light injection annealing.

Heterojunction Module Attenuation Mechanism and Improvement Strategy (II): Photoinjection Annealing Enhancement, Light and Dark Attenuation 1 Heterojunction Module Attenuation Mechanism and Improvement Strategy (II): Photoinjection Annealing Enhancement, Light and Dark Attenuation 2 Heterojunction Module Attenuation Mechanism and Improvement Strategy (II): Photoinjection Annealing Enhancement, Light and Dark Attenuation 3 SRC =

" light injection enhanced state " (metastable state B): after strong light injection annealing treatment, The P-H/B-H bond is broken in a large amount, the doping activation degree is the highest, and the efficiency reaches the peak. This is the state for which the battery efficiency is tested.

"Long-term operation steady state" (metastable state C): After the module operates under natural light and temperature cycles for a period of time, the hydrogen bond rupture and recombination reach a new dynamic equilibrium, and the efficiency stabilizes at a level slightly lower than peak value. This is the long-term benchmark state of the actual power generation of the power station. The switching relationship between the

three States is as follows: the light injection annealing pushes the cell from metastable state A to metastable state B; the long-term natural illumination and temperature cycling push the cell from A or B to metastable state C; standing in the dark will shift the cell in state C to the initial state A (dark decay), but it can be recovered after being exposed to light again.

[Technical details] The light injection annealing process accelerates the breaking process of P/B-H bonds through the combination of high light intensity (usually tens of times the standard light intensity) and appropriate temperature, and compresses the state switching that originally needs a long time of natural light immersion to be completed within a few minutes, and the effect is more significant.

Heterojunction Module Attenuation Mechanism and Improvement Strategy (II): Photoinjection Annealing Enhancement, Light and Dark Attenuation 4 SRC =

This is because the ability of hydrogen atoms to migrate by diffusion increases with temperature-the higher the temperature, The easier the hydrogen moves in the film, the easier it is to find and recombine with the activated dopant atoms, and the dark decay is accelerated. This phenomenon is also known as "dark heat decay.".

However, both ordinary dark decay and dark thermal decay are completely reversible: when the dark decay module is placed under illumination again, the photon energy breaks the recombined B-H and P-H bonds, the activity of the doped atoms is restored, and the efficiency is completely restored to the level before dark decay. This is essentially different from irreversible material aging decay. The red data in the figure below is the power change of the heterojunction module with dark attenuation at different times. The vertical arrow indicates that the module after dark attenuation has been illuminated for many times, and it can be seen that the power of the module has returned to the level before dark attenuation.

异质结组件衰减机理与改善策略(二):光注入退火增效、光照衰减与暗衰减5

Pravettoni, M., Rajput, A.S.On the metastability of silicon heterojunction solar photovoltaic

(I) Manufacturing side: Fine control

of light injection annealing process Light injection annealing is the key process before HJT components leave the factory. The goal is to push the battery from the initial state (metastable state A) to the level close to the long-term operation steady state (metastable state C). Reduce the performance gap between the factory state and the actual power generation state:

the light injection is insufficient: the P/B-H bond is not fully broken, the module is in metastable state A when leaving the factory, and it will still experience obvious efficiency fluctuations in the initial operation stage of the power plant; Excessive

light injection: the degree of doping activation is artificially increased, so that the factory test power is too high, and the deviation from the long-term operation steady state is increased, which easily leads to the customer's misjudgment of the module attenuation speed;

Through fine process control, it can ensure that the factory test power truly reflects the stable output level of the component under long-term use conditions. For the power station (II) Test end: The illumination pretreatment specification

components will continue to have dark attenuation during the dark storage period. The longer the storage time and the higher the storage temperature, the greater the deviation.". If the power test is carried out directly without any treatment, the measured power value will be significantly lower than nominal power, causing unnecessary quality disputes. The

correct way is to pretreat the component with standardized light before testing, so that it can be restored to the level of metastable C, and then measure it. This step is simple to perform, but is critical to the accuracy of the test results.

For the power plant owner and EPC party, special attention shall be paid to the following scenarios:

arrival acceptance test: the components shall be fully illuminated before the test after long-distance transportation and storage; Initial operation after

grid connection: the initial efficiency may fluctuate slightly, which is a normal metastable adjustment process, so there is no need to worry. Retest after

long-term shutdown: if the power station is shut down for a long time (such as covered by snow in winter), it is normal for the initial power to be slightly lower when it is re-connected to the grid, and it will recover naturally after illumination. Conclusion The three phenomena of

light injection annealing enhancement, white light illumination attenuation and dark attenuation seem to be independent, but actually share the same physical mechanism: the reversible combination and separation between doped atoms and hydrogen atoms in HJT thin films.

This metastability is not the defect of HJT technology, but the inherent response of heterojunction passivation contact system to light and temperature. There are three key conclusions:

dark decay is completely reversible and can be recovered by re-exposure to light, which is essentially different from irreversible material aging;

the fine control of light injection annealing process is the key to ensure the accuracy of factory power and the stability of initial power generation in power plants; Lighting pretreatment before

test is the key to avoid power measurement deviation at the operation and maintenance end, especially in the scenarios of arrival acceptance and shutdown retest.

Combined with the analysis of UV attenuation in the previous article, the performance management logic of HJT components in the whole life cycle is gradually becoming clear: only by understanding the mechanism and reversibility of various types of attenuation, can we make more accurate judgments in the selection, operation and maintenance, and testing links, and ensure the long-term stable power generation income of the power station.

All can be viewed after purchase
Correlation

Heterojunction (HJT) module accelerates its large-scale application by virtue of its comprehensive advantages such as high efficiency and low attenuation, but its unique amorphous silicon/crystalline silicon heterojunction structure also brings special sensitivity to ultraviolet radiation.

2026-11-27 15:54:52

The output power of HJT module is not a fixed value, but will fluctuate dynamically within a certain range with the illumination state and storage conditions.

2026-11-27 15:54:44

On November 26, 2026, Zhou Yuxian, President of China Cement Association, and his delegation went to Hubei to investigate the cement industry symposium held in Wuhan. Zhou Yuxian, president of China Cement Association, attended and delivered a speech. Wang Xuejun of Hubei Cement Industry Association presided over the meeting. Representatives of key enterprises such as Huaxin, Gezhouba, Queshi, Yadong, Jinglan and Jianfeng attended the meeting. Chen Berlin, Vice Secretary-General of China Cement Association, Hao Guozhu, Director of Party Construction Ministry of Culture, and Xiong Yue, Secretariat, participated in the survey, which was hosted by Queshi Group.